INCOFLUXR 4 埋弧焊剂与INCONEL 82焊丝匹配
INCOFLUXR 4 埋弧焊剂与INCONEL 82焊丝匹配
产品价格:¥1(人民币)
  • 规格:10×100目
  • 发货地:上海
  • 品牌:
  • 最小起订量:1公斤
  • 免费会员
    会员级别:试用会员
    认证类型:企业认证
    企业证件:通过认证

    商铺名称:午虎特种合金(上海)有限公司

    联系人:蔡玉兰(小姐)

    联系手机:

    固定电话:

    企业邮箱:18117348636@163.com

    联系地址:泗砖路600号

    邮编:200000

    联系我时,请说是在焊材网上看到的,谢谢!

    商品详情



      INCOFLUXR 4 埋弧焊剂

       

      INCOFLUX 4 埋弧焊剂是一种烧结焊剂,设计与INCONEL 82焊丝匹配使用,INCONEL 82焊丝是一种含铬20%的高镍合金。这种焊剂的典型应用是INCONEL600601合金、INCOLOY 800合金相互之间及它们与铁素体金属材料之间的开坡口焊接。这种焊丝和焊剂的匹配尤其适用于碳钢与不锈钢之间的焊接,因为其熔敷金属具有最优的热胀系数。这种焊剂的另一个主要应用是与INCONEL 82填充金属相匹配,在碳钢表面堆焊形成耐蚀耐氧化层。

       

      焊接参数:开坡口焊或堆焊:应用DCEP电流方式和窄焊道

       

      焊丝直径

      电流/安培

      电压/伏特

      焊接速度

      电极干伸长

      焊剂层厚度

      0.062 in

      1.6 mm

      240-290

      30-33

      8-11 in/min

      200-280mm/min

      7/8-1 in

      22-25 mm

      1/2-1 in

      13-25 mm

      0.093 in

      2.4mm

      250-300

      30-33

      8-11 in/min

      200-280mm/min

      7/8-1 in

      22-25 mm

      3/4-5/4 in

      19-32 mm

      电极摆动堆焊:应用DCEN电流方式,当焊丝直径为0.062 in时,摆动频率为50-70周/分;当焊丝直径为0.093 in时,摆动频率为35-60周/分

      0.062 in

      1.6 mm

      240-260

      32-34

      4 in/min

      100mm/min

      7/8-1 in

      22-25 mm

      1/2-1 in

      13-25 mm

      0.093 in

      2.4mm

      300-400

      34-37

      4 in/min

      100mm/min

      7/8-1 in

      22-25 mm

      3/4-5/4 in

      19-32 mm

       

      储藏和干燥条件

      焊剂密封在未开启的容器中可以无限期保存。如果焊剂暴露于潮湿环境中,可以在500oF保温烘干2小时或600oF保温烘干1小时后使用。

       

      焊剂颗粒尺寸

      泰勒制网目:10×100

       

      包装

      桶盖上带有橡胶密封垫圈的60磅聚乙烯桶密封包装

       

      The INCOFLUX 4 submerged arc welding agent is a sintering flux, which is designed to be used with INCONEL 82 welding wire. INCONEL 82 welding wire is a high nickel alloy with 20 % chromium. The typical application of this flux is INCONEL600/601 alloy, INCOLOY 800 alloy, and their welding between them and ferritic metal materials. This kind of wire and flux matching is especially suitable for welding between carbon steel and stainless steel because of its optimal thermal expansion coefficient. Another major application of this flux is the matching of the INCONEL 82 filler metal to the surface of carbon steel.

      Welding parameters: open groove welding or surfacing: apply DCEP current and narrow weld path

      Electrode dry extension flux layer thickness of wire diameter current/ampere voltage/v welding speed electrode

      0.062 in

      1.6 mm 240-290 30-33 8-11 in/min

      In 200-280 - mm/min 7/8-1

      1/2-1 in 22 to 25 mm

      13 to 25 mm

      0.093 in

      2.4mm 250-300 30-33 8-11 in/min

      In 200-280 - mm/min 7/8-1

      22-25 mm 3/4-5/4 in

      19 to 32 mm

      Electrode swing surfacing welding: the use of DCEN current mode, when the wire diameter is 0.062 in, the oscillation frequency is 50-70 weeks/min; When the wire diameter is 0.093 in, the oscillation frequency is 35-60 weeks/min

      0.062 in

      1.6 mm 240-2632-34 4 in/min

      100 mm/min in 7/8-1

      1/2-1 in 22 to 25 mm

      13 to 25 mm

      0.093 in

      2.4mm 300-400 34-37 4 in/min

      100 mm/min in 7/8-1

      22-25 mm 3/4-5/4 in

      19 to 32 mm

      Storage and drying conditions

      The flux seals can be kept indefinitely in unopened containers. If the solder is exposed to wet conditions, it can be used after an hour of thermal insulation drying for 2 hours or 600oF.

      Flux particle size

      Taylor's mesh: 10 times 100

      packaging

      The barrel cover is covered with a 60 - pound polyethylene barrel sealed with rubber gasketINCOFLUXR 4 埋弧焊剂与INCONEL 82焊丝匹配INCOFLUXR 4 埋弧焊剂与INCONEL 82焊丝匹配INCOFLUXR 4 埋弧焊剂与INCONEL 82焊丝匹配INCOFLUXR 4 埋弧焊剂与INCONEL 82焊丝匹配INCOFLUXR 4 埋弧焊剂与INCONEL 82焊丝匹配