ERCuSn-A铜合金焊丝
S 212
Sn5 Cu Rem.
Wear resistance. Argon arc welding of copper alloys and surfacing of steel.
ERCuSn-A
S 213
Sn8 Cu Rem.
Wear resistance. Argon arc welding of copper alloys and surfacing of steel.
ERCuSn-C
S 214
Al7.5 Cu Rem.
Wear and corrosion resistance. Argon arc welding of copper alloys and surfacing of steel.
ERCuAl-A1
S 215
Al9 Cu Rem.
Wear and corrosion resistance. Argon arc welding of copper alloys and surfacing of steel.
ERCuAl-A2
S 221
Cu60 Sn1 Si0.3
Melting point is about 890℃. Gas welding and carbon arc welding of brass, also braze welding of copper, steel and cast iron.
S 221F
Cu60 Sn1 Si 0.3
S221 welding rod coated with flux.
S 222
Cu58Sn0.9Si0.1
Melting point is about 880℃. Gas welding and carbon arc welding of brass, also braze welding of copper, steel and cast iron.
RBCuZn-C
S 222F
Cu58Sn0.9Si0.1
S222 welding rod coated with flux.
RBCuZn-C
S 223
Cu59 Sn0.6
Melting point is about 900℃. Braze welding of copper, steel and cast iron.
RBCuZn-A
S 224
Cu62 Si0.5
Melting point is about 905℃. Gas welding and carbon arc welding of brass, also braze welding of copper, steel and cast iron.
Copper
铜
合
金
S 225
Cu48 Ni10
Melting point is about 935℃and high strength. Braze welding of steel, nickel and carbide alloys.
RBCuZn-D
S 225F
Cu48 Ni10
S225 welding rod coated with flux.
RBCuZn-D
S 226
Cu60 Sn0.3
Melting point is about 900℃. Gas welding of brass, also braze welding of copper, steel and cast iron.
S 227
Cu58Sn0.9Ni0.5
Melting point is about 880℃. Gas welding and carbon arc welding of brass, also braze welding of copper, steel and cast iron.
RBCuZn-B
S 229
Cu55 Ni6 Mn4
Melting point is about 920℃, high strength. Braze welding of steel, nickel and hard carbide.
Aluminum alloys
铝
合
金
S 301
Al≥99.5
Good ductility and corrosion resistance. Gas welding and argon arc welding of pure aluminum.
ER1100
S 311
Si5 Al Rem.
Corrosion resistance, wide range of usage. Gas welding and argon arc welding of aluminum alloys other than high magnesium alloys.
ER4043
S 321
Mn1.3 Al Rem.
Good corrosion resistance, weldability and ductility. Gas welding and argon arc welding of aluminum alloys.
S 331
Mg5 Mn0.4
Corrosion resistance and high strength. Argon arc welding of aluminum alloys.
ER5183
耐磨性好。铜合金氩弧焊及钢的堆焊用
耐磨性好。铜合金氩弧焊及钢的堆焊用
耐磨、耐蚀。铜合金氩弧焊及钢的堆焊用
耐磨、耐蚀。铜合金氩弧焊及钢的堆焊用
Zn Rem.
熔点约890℃。黄铜气焊及碳弧焊用,也可钎焊铜、钢、铸铁
Zn Rem.
外涂焊剂的S221焊丝
Fe0.8 Zn Rem.
熔点约880℃。黄铜气焊及碳弧焊用,也可钎焊铜、钢、铸铁
Fe0.8 Zn Rem.
外涂焊剂的S222焊丝
Zn Rem.
熔点约900℃。铜、钢、铸铁钎焊用
Zn Rem.
熔点约905℃。黄铜气焊及碳弧焊用,也可钎焊铜、钢、铸铁
alloys
Zn Rem.
熔点约935℃。高强度,钎焊钢、镍及硬质合金用
Zn Rem.
外涂焊剂的S225焊丝
Si0.2 Zn Rem.
熔点约900℃。黄铜气焊用,也可钎焊铜、钢、铸铁
Si0.1 Fe0.8
Zn Rem.
熔点880℃。黄铜气焊及碳弧焊用,也可钎焊铜、钢、铸铁
Zn余
熔点约920℃。高强度,钎焊钢、镍及硬质合金用
塑性好、耐蚀。纯铝气焊、氩弧焊用
抗裂性好,通用性大。铝合金气焊、氩弧焊用。不宜用高镁合金
良好的耐蚀性、可焊性及塑性。铝合金气焊、氩弧焊用
Al Rem.
耐蚀,强度高。铝合金氩弧焊用
送丝不顺的主要原因来自于焊丝的刮削
刮削的产生是由于生产设备及焊丝的特性多造成的;
// 制造生产过程中会造成微粒或者鳞状屑沾粘在焊枪导管的内壁,导致焊丝表面的磨损,从而造成焊丝表面的刮削。
// 盘丝的绕线过程中,焊丝于焊丝的并列接触会造成焊丝碎屑剥落。
// 合金焊丝的刮屑通常会积聚在送丝导管内,但这种情况也常发生于送丝滚轮及导电嘴。
// 堵塞的送丝导管会造成焊接中止,焊道修整及零件更换等整体成本的上升