S 226 |
Cu60 Sn0.3 |
Melting point is about 900℃. Gas welding of brass, also braze welding of copper, steel and cast iron. |
||
S 227 |
Cu58Sn0.9Ni0.5 |
Melting point is about 880℃. Gas welding and carbon arc welding of brass, also braze welding of copper, steel and cast iron. |
RBCuZn-B |
|
S 229 |
Cu55 Ni6 Mn4 |
Melting point is about 920℃, high strength. Braze welding of steel, nickel and hard carbide. |
||
Aluminum alloys
铝
合
金 |
S 301 |
Al≥99.5 |
Good ductility and corrosion resistance. Gas welding and argon arc welding of pure aluminum. |
ER1100 |
S 311 |
Si5 Al Rem. |
Corrosion resistance, wide range of usage. Gas welding and argon arc welding of aluminum alloys other than high magnesium alloys. |
ER4043 |
|
S 321 |
Mn1.3 Al Rem. |
Good corrosion resistance, weldability and ductility. Gas welding and argon arc welding of aluminum alloys. |
||
S 331 |
Mg5 Mn0.4 |
Corrosion resistance and high strength. Argon arc welding of aluminum alloys. |
ER5183 |
送丝不顺的主要原因来自于焊丝的刮削
刮削的产生是由于生产设备及焊丝的特性多造成的;
// 制造生产过程中会造成微粒或者鳞状屑沾粘在焊枪导管的内壁,导致焊丝表面的磨损,从而造成焊丝表面的刮削。
// 盘丝的绕线过程中,焊丝于焊丝的并列接触会造成焊丝碎屑剥落。
// 合金焊丝的刮屑通常会积聚在送丝导管内,但这种情况也常发生于送丝滚轮及导电嘴。
// 堵塞的送丝导管会造成焊接中止,焊道修整及零件更换等整体成本的上升。