S 225F铜焊丝
Copper
铜
合
金
S 225
Cu48 Ni10
Melting point is about 935℃and high strength. Braze welding of steel, nickel and carbide alloys.
RBCuZn-D
S 225F
Cu48 Ni10
S225 welding rod coated with flux.
RBCuZn-D
S 226
Cu60 Sn0.3
Melting point is about 900℃. Gas welding of brass, also braze welding of copper, steel and cast iron.
S 227
Cu58Sn0.9Ni0.5
Melting point is about 880℃. Gas welding and carbon arc welding of brass, also braze welding of copper, steel and cast iron.
RBCuZn-B
S 229
Cu55 Ni6 Mn4
Melting point is about 920℃, high strength. Braze welding of steel, nickel and hard carbide.
Aluminum alloys
铝
合
金
S 301
Al≥99.5
Good ductility and corrosion resistance. Gas welding and argon arc welding of pure aluminum.
ER1100
S 311
Si5 Al Rem.
Corrosion resistance, wide range of usage. Gas welding and argon arc welding of aluminum alloys other than high magnesium alloys.
ER4043
S 321
Mn1.3 Al Rem.
Good corrosion resistance, weldability and ductility. Gas welding and argon arc welding of aluminum alloys.
S 331
Mg5 Mn0.4
Corrosion resistance and high strength. Argon arc welding of aluminum alloys.
ER5183
alloys
Zn Rem.
熔点约935℃。高强度,钎焊钢、镍及硬质合金用
Zn Rem.
外涂焊剂的S225焊丝
Si0.2 Zn Rem.
熔点约900℃。黄铜气焊用,也可钎焊铜、钢、铸铁
Si0.1 Fe0.8
Zn Rem.
熔点880℃。黄铜气焊及碳弧焊用,也可钎焊铜、钢、铸铁
Zn余
熔点约920℃。高强度,钎焊钢、镍及硬质合金用
塑性好、耐蚀。纯铝气焊、氩弧焊用
抗裂性好,通用性大。铝合金气焊、氩弧焊用。不宜用高镁合金
良好的耐蚀性、可焊性及塑性。铝合金气焊、氩弧焊用
Al Rem.
耐蚀,强度高。铝合金氩弧焊用
送丝不顺的主要原因来自于焊丝的刮削
刮削的产生是由于生产设备及焊丝的特性多造成的;
// 制造生产过程中会造成微粒或者鳞状屑沾粘在焊枪导管的内壁,导致焊丝表面的磨损,从而造成焊丝表面的刮削。
// 盘丝的绕线过程中,焊丝于焊丝的并列接触会造成焊丝碎屑剥落。
// 合金焊丝的刮屑通常会积聚在送丝导管内,但这种情况也常发生于送丝滚轮及导电嘴。
// 堵塞的送丝导管会造成焊接中止,焊道修整及零件更换等整体成本的上升