斯米克L307银焊条
Category | Trade-mark | Specification | Melting | Chemical | Application | Equivalent |
Copper 铜锌 | L103 | Wire & rod | 885-888 | Cu54 Zn Rem. | Brazing of copper, bronze and steel, subjected to low load. | 斯米克L307银焊条 |
L104 | Foil | 890-930 | Cu57 Mn2 | Brazing of carbide cutting tool. | 一、提高电弧燃烧的稳定性。无药皮的光焊条不容易引燃电弧。即使引燃了也不能稳定地燃烧。在焊条药皮中,一般含有钾、钠、钙等电离电位低的物质,这可以提高电弧的稳定性,保证焊接过程持续进行。 | |
Copper 铜磷 | L201 | Cast rod, wire & rod, powder | 710-800 | P7 Cu Rem. | Brazing of copper and copper alloys. | BCuP-2 |
L204 | Cast rod, wire | 640-815 | P5 Ag15 | Brazing of copper, copper alloys, silver and molybdenum etc. | BCuP-5 | |
L205 | Cast rod, wire & rod, powder | 640-800 | P6 Ag5 | Brazing of copper and copper alloys. | BCuP-3 | |
L207 | Cast rod, wire & rod | 640-770 | P7 Ag5 | Brazing of copper and copper alloys. | BCuP-7 | |
L209 | Cast rod, wire | 684-710 | P7 Ag2 | Brazing of copper and copper alloys. | BCuP-6 | |
Silver 银基 | L302 | Wire & rod | 745-775 | Ag25 Cu40 | Brazing of copper, copper alloys, steel and stainless steel etc. | |
L303 | Wire & rod | 660-725 | Ag45 Cu30 | Brazing of copper, copper alloys, steel and stainless steel etc. | BAg-5 | |
L303F | Flux coated rod | 660-725 | Ag45 Cu30 | L303 coated with flux, the same application as L303. | BAg-5 | |
L304 | Foil | 690-775 | Ag50 Cu34 | Brazing of copper, copper alloys and steel etc. | BAg-6 | |
L308 | Wire & rod | 779-780 | Ag72 Cu Rem. | Brazing of copper and nickel under vacuum or reducing protective atmosphere. | BAg-8 | |
L312 | Wire & rod | 595-605 |
| Brazing of copper, copper alloys, steel and stainless steel etc. | ||
L313 | Wire & rod | 625-635 |
| Brazing of copper, copper alloys, steel and stainless steel etc. | BAg-1a | |
L321 | Wire & rod 丝 | 615-650 |
| Brazing of copper, copper alloys, steel and stainless steel etc. | BAg-7 | |
L323 | Wire & rod | 665-755 |
| Brazing of copper, copper alloys, steel and stainless steel etc. | ||
L325 | Wire & rod | 645-685 |
| Brazing of copper, copper alloys, steel and stainless steel etc. | BAg-36 | |
L326 | Wire & rod | 650-720 |
| Brazing of copper, copper alloys, steel and stainless steel etc. | BAg-34 | |
Aluminum base 铝基 | L400 | Cast rod, wire & rod | 577-582 | Si11.5 | Brazing of aluminum and aluminum alloys. | BAlSi-4 |
L401 | Cast rod | 525-535 | Si5 Cu28 | Brazing of aluminum and aluminum alloys. | 1.CHH:中国航海产品代号 | |
Tin lead 锡铅 | L600 | Wire & rod | 183-185 | Sn60 Sb≤0.8 | Soldering of fusible metals and heat-treated part. | 60Sn |
L601 | Wire & rod | 183-227 | Sn18 Sb2 | Soldering of copper, copper alloys and galvanized iron plain sheet. | 18Sn | |
L602 | Wire & rod | 183-256 | Sn30 Sb2 | Soldering of copper, brass, copper alloys and galvanized iron plain sheet. | 30Sn | |
L603 | Wire & rod | 183-235 | Sn40 Sb2 | Soldering of copper, copper alloys, steel and zinc parts. | 40Sn | |
L604 | Wire & rod | 183-222 | Sn90 Sb≤0.15 | Soldering of copper and steel for food and medicine field. | 90Sn | |
L605 | Wire & rod | 232-240 | Ag5 Sn95 | Soldering of copper and steel for electrical and food field. | (1)药皮类型:钛型 ‖药皮主要成分 :氧化钛≥35% ‖焊接电源: 直流或交流 | |
L608 | Wire & rod | 295-305 | Sn5.5 Ag2.5 | Soldering of copper, copper alloys, steel and stainless steel. | (3)熔渣的比重应小于熔化金属的比重,凝固温度也应稍低于金属凝固温度,渣壳应易脱掉; | |
Nickel base 镍基 | L702 | Powder | 970-1000 | Cr7 B3 Si4 | Brazing of stainless steel under vacuum or protective atmosphere. | BNi-2 |
斯米克L307银焊条
(6)药皮类型:高纤维素钾型 ‖药皮主要成分 : 有机物15%以上,氧化钛30%左右 ‖焊接电源:直流或交流