英国曼彻特 ENiCrFe-3镍基焊条山东销售电话
182类合金焊接材料 | |||||
产品牌号 | 焊接方法 | 产品数据 | AWS | DIN |
|
NIMROD 132KS | MMA | 10-03C | ENiCrFe-1 | - | |
NIMROD 182KS | MMA | 10-03A | ENiCrFe-3 | EL-NiCr15FeMn | |
NIMROD 182 | MMA | 10-03A | ENiCrFe-3 | EL-NiCr15FeMn | |
NIMAX 182 | MMA | 10-03B | ENiCrFe-3 | EL-NiCr15FeMn | |
NIMROD NC19Nb | MMA | 10 | - | EL-NiCr19Nb | |
20.70.Nb | TIG/MIG/SA | 15-06A | ERNiCr3 | SG-NiCr20Nb | |
NiCr | Flux | 17-06C | - | - | |
|
|
|
|
|
|
AB类合金焊接材料 | |||||
NIMROD AKS | MMA | 10-04A | ENiCrFe-2 | EL-NiCr15MoNb |
|
NIMROD AB | MMA | 10-04A | ENiCrFe-2/4 | EL-NiCr15MoNb | |
NIMAX A | MMA | 10-04B | ENiCrFe-2 | EL-NiCr15MoNb | |
20.70.Nb | TIG/MIG/SA | 15-06A | ERNiCr-3 | SG-NiCr20Nb | |
NiCr | Flux | 17-06C | - | - | |
|
|||||
625类合金焊接材料 | |||||
NIMROD 625KS | MMA | 10-0** | ENiCrMo-3 | EL-NiCr20Mo9Nb |
|
NIMROD 625 | MMA | 10-0** | ENiCrMo-3 | EL-NiCr20Mo9Nb | |
62-50 | TIG/MIG/SA | 15-06B | ERNiCrMo-3 | SG-NiCr21Mo9Nb | |
NIMROD 721KS | MMA | 10-05E | - | - | |
72-10 | TIG/MIG/SA | 15-06N | - | - | |
|
|||||
C类合金焊接材料 |
|
|
|
|
|
NIMROD C276 | MMA | 10-07A1 | ENiCrMo-4 | EL-NiMo15Cr15EW |
|
NIMROD C276KS | MMA | 10-07A2 | ENiCrMo-4 | EL-NiMo15Cr15W | |
HAS C276 | TIG | 15-06E | ERNiCrMo-4 | SG-NiMo16Cr16W | |
NIMROD C4KS | MMA | 10-07C | ENiCrMo-7 | EL-NiMo15Cr15Ti | |
HAS C4 | TIG | 15-06H | ERNiCrMo-7 | SG-NiMo16Cr16Ti | |
NIMROD 59KS | MMA | 10-07F | ENiCrMo-13 | EL-NiCr22Mo16 | |
HAS 59 | TIG | 15-06J | ERNiCrMo-13 | SG-Ni23Mo16 | |
NIMROD C | MMA | 10 | ENiCrMo-5 | SG-Ni23Mo16 | |
|
|
|
|
|
Cr-Mo耐热焊接材料
焊条
类别 |
品名 |
AWS型号 |
焊缝金属化学成份(wt %) |
全焊缝金属机械性能 |
特征与用途 |
||||||||||||
C |
Mn |
Si |
S |
P |
Cr |
Mo |
Cu |
Sn |
As |
Sb |
抗拉强度 |
0.2%屈服强度 |
Akv冲击功 |
||||
焊条 |
Chromet 1 |
E9015-B9 |
0.07 |
0.8 |
0.3 |
0.012 |
0.015 |
1.25 |
0.55 |
<0.10 |
|
|
|
650 |
570 |
160 |
手工电弧焊条,满足AWS/ASME和BSEN标准,适用于大多数电站设备的建造 |
Chromet1L |
E7015-B2 |
0.04 |
0.8 |
0.3 |
0.012 |
0.015 |
1.25 |
0.55 |
0.05 |
|
|
|
600 |
500 |
180 |
焊缝金属硬度和焊接残余应力较低,具有优良的抗硫化物应力腐蚀开裂的性能,也适用于焊后不进行热处理的薄截面结构的焊接 |
|
Chromet 1X |
E8018-B2 |
0.04 |
0.8 |
0.3 |
0.012 |
0.015 |
1.25 |
0.55 |
<0.05 |
0.002 |
0.003 |
<0.002 |
660 |
570 |
160 |
严格控制残余有害元素,确保熔敷金属具有低的X和J脆化指数,在400-600℃的工作温度下具有优良的抗回火脆化性 |